Part Details | IRON PIG
9640-00-267-4175 A primary raw form of metal produced by pouring molten iron resulting from the blast-furance smelting down of iron ore with flux and coke, and with or without the addition of scrap iron and steel, into molds for remelting or refining use.
Alternate Parts: ASTM A43, 9640-00-267-4175, 00-267-4175, 9640002674175, 002674175
Supply Group (FSG) | NSN Assigned | NIIN | Item Name Code (INC) |
---|---|---|---|
96 | JAN 01, 1963 | 00-267-4175 | 16062 ( IRON PIG ) |
REFERENCE DRAWINGS & PICTURES
Cross Reference | NSN 9640-00-267-4175
Part Number | Cage Code | Manufacturer |
---|---|---|
ASTM A43 | 81346 | AMERICAN SOCIETY FOR TESTING ANDMATERIALS |
Technical Data | NSN 9640-00-267-4175
Characteristic | Specifications |
---|---|
COMPOSITION AND PERCENTAGE | A561097.68 MINIMUM BY VOLUME AND A92831.26 MINIMUM BY VOLUME AND A92831.50 MAXIMUM BY VOLUME |
IMPURITIES LIMITATION IN PERCENT | MANGANESE 0.75 MAX AND PHOSPHORUS 0.035 MAX NAD SULPHUR 0.035 MAX |
WEIGHT | 30.0 POUNDS MINIMUM AND 50.0 POUNDS MAXIMUM |
SPECIAL FEATURES | GADE LP4 |
SPECIFICATION/STANDARD DATA | 81346-STM 43 PROFESSIONAL/INDUSTRIAL ASSOCIATION SPECIFICATION |